Bamboo Flooring Settings for Wagner Meters Handheld Moisture Meters

Below you will find specific gravity settings for bamboo flooring products from the following manufacturers:

  1. Teragren®
  2. Wellmade® Performance Floors
  3. Cali Bamboo

 

Settings* for Teragren® Bamboo Flooring Products

MATERIAL DESCRIPTIONTERAGREN® PART NO.SETTING
Stranded Wheat-Color, Not CarbonizedTPF-SYN-WHT-MPL0.97
Traditional (not-stranded) Flat-grain, carbonizedPF-FGC-MPL0.97
Stranded, Chestnut, carbonizedTPF-SYN-CHSNT-MPL1.0
Traditional (not-stranded) Vertical-grain, carbonizedPF-VGC-MPL0.66
Traditional (not-stranded), Flat-grain, not-carbonizedPF-FGN-MPL0.69

 

Settings* for Wellmade® Performance Floors Bamboo Flooring Products

MATERIAL DESCRIPTIONWELLMADE PART NO.SETTING
Solid Strand Bamboo (Natural )STRCLKN12101.0
Solid Strand Bamboo (Carbonized)STRCLKC12101.0
Solid Strand Bamboo (Ebony)STRCKLKEBO1.0
Engineered Strand (Carbonized)CARB-ES .68
Engineered Strand (Natural)NAT-ES4 .67
Engineered Strand (Walnut)WALHS-ES4 .71

 

Settings* for Cali Bamboo Flooring Products

ProductOptimum Setting
Natural Fossilized Bamboo Flooring 14 mm1.0
Carbonized Fossilized Bamboo Flooring 14 mm1.0
Engineered Fossilized Natural Bamboo Flooring 14 mm0.83
Engineered Fossilized Carbonized Bamboo Flooring 14 mm0.82
Eucalyptus Fossilized Natural Flooring 14 mm1.0
Eucalyptus Fossilized Carbonized Flooring 14 mm1.0
Carbonized Fossilized Bamboo Flooring 11 mm0.96
Natural Fossilized Bamboo Flooring 11 mm0.87

*These settings were derived from sample populations of the different flooring products provided by the above manufacturers. These samples were lab-tested for actual moisture content at Wagner Meters using the ASTM D4442-92 oven-dry method. The oven-dry results were then used to establish the optimum settings for Wagner Meters digital handheld moisture meters.

ASTM D4442-92 is the laboratory standard method used to verify the level of accuracy of handheld moisture meters for wood.

Decimal point is not shown on the meter display. Example: when setting your meter for .59, the actual value on the meter display will be 59.