The Pros & Cons of Tigerwood Flooring & Tigerwood Decking
Discover the beauty and benefits of Tigerwood, a striking and resilient exotic hardwood perfect for your flooring and decking needs. With its unique blend of dramatic grain patterns and rich reddish-orange tones, Tigerwood adds a touch of luxury to any space.

In this article, we’ll explore the following:
- What Is Tigerwood?
- What is Tigerwood Used For?
- Working with Tigerwood Lumber
- Tigerwoodâs Pros
- Tigerwoodâs Cons
- Tips to Maintain Tigerwood Flooring and Decking
- Tigerwood Durability
- Moisture Content in Tigerwood
- FAQs
What Is Tigerwood?
Tigerwood is a durable and dramatic exotic wood species known for its dark vein stripes and beautiful deep reddish-orange background.
Tigerwood is also known by a variety of names, including:
Brazilian koa, Congo wood, African walnut, Courbaril, Bototo, Zorrowood, and Muiracatiara.
When someone uses the term âtigerwood,” they may be referring to Coula edulis, a tree species from tropical western Africa, Lovoa trichilioides (also African in origin), or Goncalo alves from South America (primarily Brazil).
These are all evergreen varieties that prefer tropical or subtropical growing conditions. Although the color may vary from region to region, these tigerwood trees all feature the same dramatic grain pattern.
Because tigerwood trees can reach over 80 feet, theyâre often found in the top forest canopy. However, they can also be found on lower canopies as well. They have no special soil requirements, and their growing popularity has led some countries to restrict exports to limit over-cutting.
Tigerwood Characteristics
Tigerwood is very dense and heavy and can have a Janka rating of up to 2160 depending on the growing region. This is 67% harder than red oak, which only has a Janka rating of 1210.
Because tigerwood is naturally resistant to rot and decay and doesnât attract mold or fungus growth, itâs popular not only for exterior use but also for furniture, veneers, flooring, and other wood projects. Its dramatic look lends a certain flair to finished products.
Tigerwood responds well to air-drying even though warping and checking can occur under extreme conditions. After it has dried, itâs resistant to both shrinkage and movement.
Projects made from tigerwood are dimensionally stable and hold up well.
Brazilian Tigerwood is known for its beautiful colors â from light orange down to a deep reddish-brown â and striping, which varies from fine lines to bold strokes. Its highly lustrous surface makes it look almost oily.
Because Brazilian hardwood is highly durable and resists denting, itâs often used for flooring. Its dramatic coloring means itâs often graded differently from other hardwood species for flooring applications. It has small defects and less striking variations in color are graded as âcommon.â
Tigerwood, graded as âclear,â has deep black or brown stripes and a deep orange base color with a hint of pink.
What is Tigerwood Used For?
Tigerwood hardwood is often used for interior flooring, musical instruments, and fine furniture. Its durability and water-resistant qualities also make it perfect for anything used outdoors, including outdoor deck boards, shutters, deck furniture, and boats. It is also used for decorative items because of its beautiful grain patterns.
Working with Tigerwood Lumber
Tigerwood is considered only moderately difficult to work with despite its hardness if you have professional hand tools. Because cutting edges may wear down more quickly than other wood species, carbide tips or bits are recommended. We also recommend drilling before using screws or nails on tigerwood.
Because it can be a challenge to sand this hard, exotic wood, we recommend professional preparation when using it for large applications such as flooring.
Tigerwood can be sealed for increased durability but weathers well naturally, without preservatives. Sunlight changes the color of the wood. Some people have observed the wood getting darker. Others report that it gets lighter.
Tigerwoodâs Pros
1. Tigerwood is durable
With a Janka rating of 2160, Tigerwood is harder than many other kinds of wood. That makes it good for flooring and decking, which gets a lot of heavy use. For example, families with children and dogs.
2. Beautiful and unique
It gets its name from the dark, pretty âtigerâ stripes of varying thicknesses and rich reddish-orange base.
3. Water-resistant
Tigerwoodâs density and natural oils make it resistant to water. Therefore, itâs good for damp environments like decks and outdoor furniture.
4. Exotic, but not too pricey
Exotic hardwoods can be very expensive. Tigerwood is exotic, durable, and resists moisture but wonât break your budget.
5. Easy to maintain
Maintaining the wood is easy. All you need is a dust mop or vacuum cleaner. For deeper cleaning, mix Âź cup of mild soap in 2 gallons of water, and youâll be able to wash away dirt without harming the finish. Whatever you do, donât use a cleaner thatâs not designed for exotic hardwoods.
Tigerwoodâs Cons
1. The color of tigerwood will change over time
Tigerwood starts with high contrast between the various colors. However, the lighter colors will slowly darken over time, making this contrast less noticeable. You can slow this down by limiting the amount of sunlight the floor gets.
2. Grows in rainforests
While tigerwood is not an endangered species, there are concerns about over-logging. Some tigerwood-growing countries â including Brazil, where most US tigerwood comes from â have placed export restrictions on it to prevent over-cutting.
3. Donât try this yourself
Tigerwood is hard. Therefore, it will not be a DIY project for many people. Youâll need professional tools such as saws with carbon-tipped blades and carbide bit drills to create pre-drilled holes for nails and screws. It also isnât easy to glue because of the natural oils in the wood.
Tigerwood is a show-stealer. Its warm, striking coloring can turn any floor into a centerpiece. Its hard, durable nature makes it perfect for various uses, including, but not limited to, flooring, decks, and fine furniture.

Tips to Maintain Tigerwood Flooring and Decking
Caring for Tigerwood Flooring
Caring for tigerwood flooring is relatively easy. There are just a few things you should keep in mindâŚ
- Keep tigerwood flooring clean. Be sure to vacuum or sweep up any visible dust or dirt.
- Clean up liquid spills immediately.
- Use rugs in areas with a lot of foot traffic.
- Use felt pads under furniture legs.
- Keep your petâs nails short.
- Avoid rugs with a rubber backing as they can cause the area underneath them to fade.
- Try to avoid having the sun beat down on the same area of the floor every day.
- Rearrange your furniture periodically so the tigerwood floor can change color (i.e., age) consistently.
Caring for Tigerwood Decks
Left on its own, it will naturally age and take on a beautiful, rustic gray color. Clear sealers will protect your deck boards from dirt and rain. However, they canât stop the color from fading. If thatâs OK with you, use a simple, clear sealer.
Select a lighter stain if you want some of the woodâs natural color to show through. Your deckingâs location and how much use it gets will determine how often youâll need to apply a new coat. If you start to see fading, itâs time for another stain application.
Clean your tigerwood decking regularly with mild soap and water or just water for a quick rinse. Dirt acts as an abrasive and can damage the surface of the wood. Pollen is also a problem because it can lead to mold growth, leading to rot. It only takes a few minutes of TLC to preserve your investment.

Free Download – Wood Flooring Installation: What To Expect
Tigerwood Durability
The Janka hardness test measures a woodâs durability using a small steel ball to determine the amount of force necessary to dent the surface of the wood. Species that can withstand more pressure before denting have a higher Janka rating, while softer woods have a lower rating.
What is the Hardest Wood
Tigerwoodâs Janka hardness scale rating of 2160 makes it harder than many other durable wood species. Itâs twice as hard as Peruvian Walnut, which has a Janka rating of 1080 but is slightly softer than Brazilian Cherry, with a hardness scale rating of 2350.
Is Tigerwood Good for Flooring?
Yes, because tigerwood is highly durable. Its density makes it resistant to water, bugs, and rot. If properly maintained, it can last for over 50 years if used in interior locations and over 25 years if used outside. This makes it a great wood for both interior flooring and outside decks.
Moisture Content in Tigerwood
As with all wood species, managing the moisture content of tigerwood is crucial if we want to protect our projects…
Tigerwood is typically dried to a relatively low moisture content for flooring applications. However, as with any wood or wood product, the wood needs to have reached its equilibrium moisture content (EMC) before itâs used in construction to avoid moisture-related problems.
This is especially true with exotic species of wood that grow in natural environments very different from where theyâll eventually be used.
A quality wood moisture meter is the best way to accurately measure the moisture content of wood and monitor its equilibration to the surrounding environment. Our OrionÂŽ 930 Dual Depth Pinless Moisture Meter has programmable specific gravity (SG) settings for both standard domestic kinds of wood and exotic woods. It can quickly and accurately measure the moisture content in unfinished, raw lumber, and finished wood projects.
It can be summed up in just one sentenceâŚ
Accurately measuring wood moisture content at every stage during the construction of a project helps you ensure its success.
FAQs
Is Tigerwood flooring suitable for underfloor heating systems?
Yes, Tigerwood flooring can be used with underfloor heating systems. However, it’s essential to follow the manufacturer’s recommendations for installation and maintenance to ensure proper performance and prevent issues related to moisture or temperature fluctuations.
How does Tigerwood’s cost compare to other hardwood flooring options?
Tigerwood is generally more expensive than domestic hardwoods like oak or maple but is typically less expensive than other exotic hardwoods like Ipe or Brazilian Cherry.
Understanding the nuances between sapwood and heartwood is crucial for anyone working with wood. Delve into our detailed piece, ‘Sapwood and Heartwood â What Are The Differences,’ to enhance your selection process and ensure the success of your woodworking endeavors.
Larry Loffer is a senior technician at Wagner Meters, where he has over 30 years of experience in wood moisture measurement. With a degree in Computer Systems, Larry is involved in both hardware and software development of wood moisture measurement solutions.
Last updated on December 11th, 2024





Larry
We really need your sage advice. We have a large deck about 60 feet long and at least 12 feet wide. Last year I tore up 25 year old painted pressure treated wood and installed Tigerwood. It was “clipped down at the edges so there are no nails or screws. We lives on a golf course in Virginia and under a canopy of of Oaks and Poplars and Dogwoods adjacent to the Par 5 of number 8. Over the past year I have noticed a black coating and a couple of areas of fungus near the Weber Gas Grill which might be spillage from grilling. My question is what would you suggest I use to clean the deck on what may be an annual spring exercise? One contractor said to power wash it with soap and water and another said use Xylene and another said the CLR solution. All seem a little drastic when all I really want to do is clean the tree sap and pollen. The wood is expensive and visually beautiful as you know and I want to be very careful. Last question, since it is a year old do I need to reseal it and if so, with what? Give me your best advice and shirt size and I will send you one of our golf shirts.
Many thanks
Tim
Tim,
It isnât clear if the âBlack coatingâ is mold due to moisture, or if itâs drips from the grill.
If the problem is high moisture in the wood, the first step is to remove the mold and check the Tigerwood using a moisture meter. https://www.wagnermeters.com/moisture-meters/comparison-matrix/
Mold begins to grow when the moisture content is about 25% and above.
Cover the area from precipitation and allow to dry.
Once dried, check with your Tigerwood supplier for their recommended sealer.
We just installed a Brazilian Tiger Wood deck. Some of the planks have developed spits, cracks on the ends. We are being told this is ânormal and typical â even though it is sporadic. Is this from poorly kilned wood or is it to be expected?
Hi Wade,
Several factors can cause checking on the ends of boards. You named one of them improper kiln drying. Also, if your relative humidity is low, this will cause wood to shrink, and thus crack. Your best bet now is to apply a sealer so it doesn’t get worse. Inquire at your local home store.
all kinds of materials used for flooring have their own pros and cons but tigerwood flooring suits best for our deck. One of the main reasons is it’s water-resistant.
You would have to restain the whole floor. I too have a Brazilian tiger wood deck thatâs now 12 years old. Iâve learned the lesson about circular sanders as well and whoever sanded your floors is no pro. Any wood thatâs darker will leave sanding swirls. Itâs common sense. Hereâs what I would do in your situation: wait for the swirls to fade.. period.. they will fade too. Give your floor two months and it will blend eventually. If youâre worried about those pimples in the poly which I would be.. you can get like a really light sandpaper.. like 200 grit+ And sand the pimples down lightly.. then recover it with a swipe or two of sealant.
Can you use rubber rug pads with holes in them on tiger wood?
Abby,
I would double-check with the manufacturer of the tiger wood and underlay. Unfortunately, that isnât something we can easily answer.
I, too, aquired some tigerwood that I would like to use for knife handles. Any comments?
Hi,
We had wood tigerwood installed in our home 15 years ago.
I would like to have the floors refinished and am wondering if they could be stained a darker colour.
Thank you!
Hi Tracey,
Yes, your floors can be stained a darker color.
Hi I have Brazilian tiger wood floors that were sanded and sealed and I can see the circular motions of the sander … I also see many âpimples â in the poly . Iâm so disappointed. Also my floors look very orange. I donât like it. Whatâs the fastest way to get them darker ? Ty
Hi,
I am looking to redue my deck in tiger wood slats 5/4 x 4 slats, railing and stairs. would you have the wood to complete my project?
thank you .
Hi Sherry,
We don’t sell wood. We only sell moisture measurement products such as wood moisture meters. Maybe check with Homedepot or if you have a local hardware store you go to.
We have tiger wood throughout our home. The sun is fading an area in the kitchen. I am perplexed as I thought sun would darken the floor.
Anything we can do to prevent the fading or remedy the existing fading?
Previous owners used a rug and the floor is darker under the rug.
Thank you in advance.
Pat,
Iâm sorry to hear about your floor! I love Tigerwood!
Area rugs and non-slip area rug pads that are incompatible with the wood floor finish systems or have been placed over uncured finishes can leave discoloring stains, blushing of the finishes, or impressions in the finish as well as the wood.
Having exposure to the sun can cause fading, bleaching, and darkening of the wood in your flooring.
There are 3 types of light that can cause this. One is ultraviolet (UV) light. Another is visible light. The last is infrared light (IR).
Minimizing the exposure to light will help, but a sand & recoat my be needed. Thanks for reaching out, I hope this was helpful.
Have a tigerwood deck installed last summer, it’s cried, we sanded and stained, thinking needs another coat of stain, soaked in fast, but wondering about a water sealer.. Does it need one? Like the high glossy look stain too.. Is it OK to use that?
Lydia,
Thank you very much for writing in on your deck. Decks can be difficult to keep maintained: particularly with varying outside weather conditions. The manufacture of the decking, or company you purchased it from should be able to direct you towards a product they recommend for your deck.
Thanks again for writing us, best of luck!
I will be making a dining room table out of Goncalo Alves. I know I am suppose to wipe the wood down with a solvent before gluing, but do I also need to do this before finishing?
I have engineered Bruce Tigerood installed in our house. We have a dog that has left some deep scratches on portions of the floors. We have area rugs in three of the rooms so their is just some deep scratches around the edges that the rugs did not cover and the stairs going up to the second level. Can anything be done to just repair the deep scratches without doing al the floors? The areas covered are in pristine shape.
Thanks
Sharron
You should contact the company that installed the floor to get a recommendation on trying to refinish/repair. Also, here is a link to an article that may help you: https://www.builddirect.com/learning-center/flooring/how-to-fix-scratches-on-engineered-hardwood-floors/
I put area rugs on newly laid tigerwood floors 4 years ago before they darkened. How do I now darken them to match? Can they be stained or refinished somehow?
Margaret:
Thanks for the question. Depending on how bad the situation is you may be able to rotate the rugs to other areas of the house, allowing the lighter areas to be exposed to the UV. Doing this may darken the wood helping to blend the variations. You may also be able to sand and refinish depending on how deep the discoloration penetrates the wood. Contact a qualified sand and finish professional in your area. Good luck.
We are planning to put tiger wood for ceiling underneath front porch and lanai in a new construction home
Will this work and if so do I need to seal it? I live in southern Georgia where we have hot summers and sometimes cold winters. It wonât have direct sunlight
Thanks for your help
Gene
Gene:
Thanks for the questions. It looks like Tigerwood is lauded as being very dimensionally stable which is what you are most concerned about in this application. This being said, I would still consult a local professional to verify this and get there opinion prior to proceeding. Good luck.
We had a tiger wood deck installed last year and they put varnish on it which is now peeling.
What’s the best way to clean it off and refinish the wood?
Nancy:
Thanks for the questions. Sometimes, depending on how loose the varnish is, you can just power wash, but in other cases, you may have to sand. I would find the product you are going to use to refinish the deck and consult them for proper preparation in order to use their product effectively.
We have a tigerwood floor on our front porch. It was gray. We cleaned and then used sander preparing the wood for a protective water shield. Using the sander caused several dents in the floor. Do you have a suggestion on how to fill those, etc.
Thanks you.
Pam Everette
Pamela:
Thanks for the question. When you say âdentâ I am going to assume you mean areas where the sander got away from you and sanded too much wood. This tends to be a common issue if you arenât intimately familiar with sanding equipment and the sanding process. In this situation, most would say the best way to help this is to blend the affected area, or sand it so its not so drastic and noticeable. Depending on the situation, this may also be an option https://www.hunker.com/13415140/how-to-repair-a-deck-with-wood-filler
Hello,
I am currently looking for samples of Tigerwood to use for knife handles. How could I go about finding a source of this tigerwood? Would there be an installer that deal in this that i could get some of the unused cuttings from?
Hi Larry,
I am looking at Tigerwood vs composite material for a deck project. This new deck project is only steps from the ocean. It will be exposed to salt spray and during a big storm it will get hit with salt water. Do you see a problem with that?
Sincerely,
John
Tigerwood decking is naturally resistant to rot and decay and usually has a 25-year plus life span. This makes it a great choice for decking. Saltwater or spray should not have much impact on the life of the deck. However, over time, the salt environment will probably have an effect on the look of the deck and it will show weathering unless it is stained and also cleaned on a regular basis. Oil-based deck stains with a UV inhibitor are the best choice for slowing the weathering process.
Hi Larry,
My husband and I are building a house in upstate NY. The temps range from minus 20 Fahrenheit in the winters and about 100 F in the summers. We are using Tigerwood decking as an accent to the siding we are putting up. Do you have any information on how Tigerwood ages and the best species to use for this?
Best, Samantha
Hi Samantha,
Solid Tigerwood is an expensive exotic hardwood that is normally used indoors, in a temperature controlled environment, for flooring or furniture. There are engineered Tigerwood products that are designed for siding. Just make sure that it is rated for your extreme temperatures.
Larry,
Can you lay tiger flooring over radiant floor heating. It is the hot water radiant in concrete. Would like to use this flooring but are getting mixed responses on this.
Cheryl:
Thanks for the question. This is a better question posed to the specific flooring manufacturer you will be using for your floor. In general, I have heard of many different species being used over radiant heat without issue. Good luck.
Hi Larry,
We recently purchased a new home in Omaha with tiger wood throughout the main level. We have a humidifier set to 35% – is there a recommended humidity range specific to tiger wood? Thanks Larry!
Larry,
There isnât a special humidity level for tiger wood that I know of.
You will want to keep the same percent humidity level when the floor was installed.
In other words, if the flooring was equilibrated to 40% humidity when installed, you will want to keep the same humidity level. This will keep the tiger wood from shrinking or swelling.
Larry I have an old rocking chair that is tiger wood. I have to refinish it. What do I use to treat it?
Hi Charlene,
Re-finishing isnât my strong point. I did find some good articles:
First, make sure the chair is worth re-finishing:
https://www.diynetwork.com/how-to/make-and-decorate/decorating/how-to-tell-if-wood-furniture-is-worth-refinishing
Here is a good link to re-finishing tropical hardwoods. The Wood Database is a good reference we use frequently:
https://www.wood-database.com/wood-articles/finishing-exotic-tropical-hardwoods/
Hello Larry,
I have an engineered tigerwood floor. Still, after 5 years, it still has a wood odor especially strong at 80 degrees. The first month after installation, I had a severe reaction to the outgassing even though I was told there were no VOC’s. I am chemically sensitive and I do not know what to do as I feel it is adversely affecting my health. I am keeping the temperature in the house lower but it is still somehow outgassing. I would very much appreciate your advice.
Thank you,
Hi Stuart,
If you are certain the outgassing is coming from the Tigerwood, perhaps a layer of some type of sealer or lacquer will do the trick. This should seal in the emissions.
Hi Larry, we have had tiger wood in our garage for 3 weeks prior to starting an interior flooring project. We laid 6 planks and then decided to measure moisture content. Our sub floor is 8 and the tiger wood ranges from 13 to 21%. After discovering this we brought as much into the house as possible. The moisture content is barely changing. Do you know how long we can expect it to take? We are keeping the house (new construction) at about 70 degrees. How do I calculate EMC? I need to know when my wood has reached it.
Hi Jodi,
My first concern is that you have the right setting/correction factor for Tigerwood for your moisture meter.
If you are using one of ours, the SG setting is .85.
Second, we have a free APP called âWoodH2Oâ. It can be downloaded for either an iPhone or Android.
This APP has a function that will give you the EMC.
Larry,
I am installing albino rhino tigerwood. What is the best type of sealer that will not darken the colors of the wood. Also, is it necessary to even seal this? This will be placed through out the main floor.
Hi Chris,
Wood sealing is a little out of my range of expertise. I know finishing exotic oily woods can be tricky. Here are a couple links to help you;
http://www.wood-database.com/wood-articles/finishing-exotic-tropical-hardwoods/
https://www.thewoodwhisperer.com/articles/finishing-oily-woods/
Thank you
I am installing tiger wood on my deck do I need to preserve this wood due to exterior conditions. I live in the Upstate of SC ?
Hi Diana,
Yes, all species of wood needs protection when exposed to the elements.
This is a good guide for Tigerwood deck care: http://homeguides.sfgate.com/caring-tigerwood-deck-39769.html
Larry I have arcadia tiger wood floor. My house was just flooded. Part of the wood needs to be replaced. Do I have to pull up all the flooring in the house? I’m worrying about it all matching.
Hi Charmaine,
Since you mentioned a flood all the flooring will need to be removed and the sub-floor examined.
If you had an appliance leak, then only part of the floor would need to be replaced/examined.
Mold is a concern if all of the moisture isnât removed.
Hi there, our flooring is only two years old. I’ve babied this flooring but it has what looks like water marks all over it. I’m beside myself. The floors look great for the first day after cleaning but the marks return and it looks terrible. Almost like the finish has been damaged. The only think i can think of was that my mop head had somethinh on it. It litterly happened over night. Is there anything I can apply to it to bring back its original luster.
Hi Jo,
Is there any cupping or warping of the individual boards?
If not, this doesnât sound like a moisture related issue.
I would start by contacting the National Wood Flooring Association (NWFA).
Their Website is
https://www.nwfa.org/
Another good resource is:
https://www.familyhandyman.com/floor/hardwood-floors/how-to-refinish-hardwood-floors/view-all/
Thank you
Hi,
We are installing Tigerwood rainsiding in an atrium. The longest lengths being 12â. What precautions should we take when butting the the inside corners. We would like a seamless look but living in Phoenix wonder about the expansion and contraction. Installing in 60 degrees but can reach up to 120. Any suggestions?
Thanks
Mark
Hi Mark,
The answer depends on the relative humidity that may change, such as from season to season. If this is a controlled environment that can be kept at constant humidity, then you can get away with butting the pieces together.
What concerns me is the wide swing in temperature. This usually means quite a change in humidity as well.
I would leave space in this situation just in case.
I find that my tiger wood floors are very prone to denting and yet I had it installed because of it’s hardness. I’m disappointed.
The Janka hardness (a test that measures the resistance of a sample of wood to denting and wear) varies greatly for the different species known as Tigerwood. For example, Lovoa trichilioides measures about 940, while Goncalo Alves can have a hardness of up to 2160 (red oak is typically around 1120).
Since Tigerwood is a generic name for multiple species, knowing which Tigerwood species you are having installed can make a world of difference when it comes to denting and wear resistance.
Hi Larry,
Thanks for your informative notes on Tiger wood. In the Philippines, woodworkers will call a type of tree Tiger wood, and I’ve always wondered what tree it really is. Recently I saw the inside of the Philippine Tiger wood. The colors of your samples seem to match the colors I’ve seen in the Tiger wood in the Philippines. My question is, do you know if Tiger wood grows in the Philippines?
Thanks!
I am unaware of any Tigerwood grown in the Philippines, the majority of commercial Tigerwood comes from South America (primarily Brazil).
Can you match tiger wood, if half floor was damaged..??
Since there are many wood species known as Tigerwood, without knowing the exact species and where it came from, it would be extremely difficult to match a pre-existing floor. You might try contacting a company that specializes in Tigerwood products to see if the flooring can be matched.
How can you bleach this wood to lightin it. I have tried A B bleach but little to no color change
Hi Bryan,
Not sure why you would want to bleach an exotic hardwood such as Tigerwood but please search the web for âBleaching wood grainâ.
Here is a good example: https://www.bobvila.com/articles/bleaching-wood/
Thank you
Hi Larry!
I’m renovating an old kitchen in Sydney. And stripped the skirting boards to find a real tiger-like pattern on the wood. I looked it up and suspect it is Tasmanian Tiger Myrtle. But it could be anything – I realised after reading your info.Thanks.